Description
Sr. No. | Property General | Unit | Test Method | Typical Values | ||||||||
1 | Thickness | Micron | Polymers | 12 | 15 | 19 | 25 | 30 | 36 | 50 | 75 | 100 |
2 | Yield | M2/Kg | Polymers | 59.5 | 47.6 | 37.8 | 31 | 23.8 | 19.8 | 14.3 | 9.5 | 7.14 |
3 | Density | gm/cc | ASTM-D-1505 | 1.4 | 1.4 | 1.4 | 1.4 | 1.4 | 1.4 | 1.4 | 1.4 | 1.4 |
4 | Water Absorption (Max) | % | ASTM-D-1505 | 0.8 | 0.8 | 0.8 | 0.8 | 0.8 | 0.8 | 0.8 | 0.8 | 0.8 |
Thermal | ||||||||||||
1 | Shrinkage @150°C 30 Min | ASTM-D-1204 | ||||||||||
MD | % | 2 | 1.6 | 1.6 | 1.6 | 1.6 | 1.6 | 1.2 | 1 | 1 | ||
TD | % | 1 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | ||
2 | Melting Point | °C | DSC | 255 | 255 | 255 | 255 | 255 | 255 | 255 | 255 | 255 |
Mechanical | ||||||||||||
1 | Tensile Strength | Kg/Cm2 | ASTM-D-882 | 1800 | 1800 | 1800 | 1800 | 1800 | 1800 | 1800 | 1800 | 1700 |
2 | Elongation (MD/TD) | % | ASTM-D-882 | 90 | 90 | 90 | 100 | 100 | 100 | 130 | 140 | 150 |
3 | Slip (COF) | ASTM-D-1894 | 0.5 | 0.5 | 0.5 | 0.5 | 0.5 | 0.4 | 0.4 | 0.3 | 0.3 | |
Optical | ||||||||||||
1 | Haze | % | ASTM-D-1003 | 3.5 | 4 | 4.5 | 5 | 6 | 8 | 10 | 10 | 10 |